DSC (Differential scanning calorimetry)
DSC is a thermal analysis apparatus measuring how physical properties of a sample change, along with temperature against time. In other words, the device is a thermal analysis instrument that determines the temperature and heat flow associated with material transitions as a function of time and temperature.

Specifications
- Temperature Range: Amb to 725 ˚C
- With Cooling Accessories: -180 to 725 ˚C
- Temperature Accuracy: +/- 0.1 ˚C
- Temperature Precision: +/- 0.05 ˚C
- Calorimetric Reproducibility(indium metal):+/- 1 %
- Calorimetric Precision (indium metal): +/- 0.1 %
- Dynamic Measurement Range: +/- 350 mW
- Digital Resolution: >0.04μW
- Baseline Curvature (-50 to 300 ˚C) : <0.15mW
- Baseline Reproducibility: < 0.04 mW
- Sensitivity 1.0 μW
- Indium Height / Width (mW/˚C)* 8.0

Control Modes - Heat flow
What data we get?
- Onset of Decomposition temperature
- Endothermic event
- Melting /Phase change event
- Heat of reaction
- Glass transition temperature